Stick Welding Tips, Certification tests, machines, projects
I have a job coming up soon that will require me to weld outside in below freezing temperatures, will I need to warm up the base metals before welding?
Lincoln 225 ac buzz box(my first machine)
farmhand 110 vac mig/fluxcore
miller aead 200le
farmhand 110 vac mig/fluxcore
miller aead 200le
- Otto Nobedder
-
Weldmonger
-
Posts:
-
Joined:Thu Jan 06, 2011 11:40 pm
-
Location:Near New Orleans
That depends a great deal on what you're welding.
I've built powerplants and ethanol plants in the freezing cold and never needed to preheat anything. Carbon steel and most 300-series stainless steels won't care if you preheat, and I've done them MIG, TIG, and stick, at down to 22 below.
Aluminum depends on the thickness and the power you have available, but preheat is always good with aluminum, even in warm weather.
The job should have a WPS for the welds. If preheat is not specified, it's not needed.'
Where and what's the job? (State is fine, if you can't post the specific job)
Steve S
I've built powerplants and ethanol plants in the freezing cold and never needed to preheat anything. Carbon steel and most 300-series stainless steels won't care if you preheat, and I've done them MIG, TIG, and stick, at down to 22 below.
Aluminum depends on the thickness and the power you have available, but preheat is always good with aluminum, even in warm weather.
The job should have a WPS for the welds. If preheat is not specified, it's not needed.'
Where and what's the job? (State is fine, if you can't post the specific job)
Steve S
actually finishing a job I started a couple weeks ago. I am welding a dump truck hoist saddle together on the frame, I have already welded the bed to the frame a couple weeks ago. there is no garage to work in and it is in Ohio.
Lincoln 225 ac buzz box(my first machine)
farmhand 110 vac mig/fluxcore
miller aead 200le
farmhand 110 vac mig/fluxcore
miller aead 200le
- Otto Nobedder
-
Weldmonger
-
Posts:
-
Joined:Thu Jan 06, 2011 11:40 pm
-
Location:Near New Orleans
For that kind of welding, all carbon steel (7018, I presume?) preheat is not an issue. For carbon steel, the difference between 100* and 10* is meaningless.
Steve S
Steve S
- Otto Nobedder
-
Weldmonger
-
Posts:
-
Joined:Thu Jan 06, 2011 11:40 pm
-
Location:Near New Orleans
I will say this...
If they'll "let" you pre-heat, it's more comfortable in cold weather...
Steve S
If they'll "let" you pre-heat, it's more comfortable in cold weather...
Steve S
well there will be some torch cutting before the welding so I will weld it before it cools completely. thanks again
Lincoln 225 ac buzz box(my first machine)
farmhand 110 vac mig/fluxcore
miller aead 200le
farmhand 110 vac mig/fluxcore
miller aead 200le
jwmacawful
- jwmacawful
-
Heavy Hitter
-
Posts:
-
Joined:Fri Aug 13, 2010 1:23 pm
-
Location:the city that never sleeps
many years ago i was working on a high rise and the welding inspector required me to preheat. not knowing any better i asked him why this was necessary. he took the propane heating torch out of my hands lit it and ran it quickly once or twice over the column i was getting ready to splice. the water that ran off and beaded up on the surface surprised me even though it wasn't visible.
- Otto Nobedder
-
Weldmonger
-
Posts:
-
Joined:Thu Jan 06, 2011 11:40 pm
-
Location:Near New Orleans
On cold steel, all that condensation came from the flame itself. The vapor from that propane flame is CO2 and H2O (water vapor), and the water instantly condenses on the cold steel. You didn't melt some invisible film of ice. He impressed a young you with his demonstration, and you did it his way.jwmacawful wrote:many years ago i was working on a high rise and the welding inspector required me to preheat. not knowing any better i asked him why this was necessary. he took the propane heating torch out of my hands lit it and ran it quickly once or twice over the column i was getting ready to splice. the water that ran off and beaded up on the surface surprised me even though it wasn't visible.
The only stuff I've seen preheated (other than ice/snow removal), even in a record cold IA winter, was the high-chrome steel and the aluminum.
Steve S
jwmacawful
- jwmacawful
-
Heavy Hitter
-
Posts:
-
Joined:Fri Aug 13, 2010 1:23 pm
-
Location:the city that never sleeps
it was summer.Otto Nobedder wrote:On cold steel, all that condensation came from the flame itself. The vapor from that propane flame is CO2 and H2O (water vapor), and the water instantly condenses on the cold steel. You didn't melt some invisible film of ice. He impressed a young you with his demonstration, and you did it his way.jwmacawful wrote:many years ago i was working on a high rise and the welding inspector required me to preheat. not knowing any better i asked him why this was necessary. he took the propane heating torch out of my hands lit it and ran it quickly once or twice over the column i was getting ready to splice. the water that ran off and beaded up on the surface surprised me even though it wasn't visible.
The only stuff I've seen preheated (other than ice/snow removal), even in a record cold IA winter, was the high-chrome steel and the aluminum.
Steve S
jwmacawful
- jwmacawful
-
Heavy Hitter
-
Posts:
-
Joined:Fri Aug 13, 2010 1:23 pm
-
Location:the city that never sleeps
column pre-heat. summertime.
- Attachments
-
- selected pics 2012 012.jpg (34.42 KiB) Viewed 2573 times
- Otto Nobedder
-
Weldmonger
-
Posts:
-
Joined:Thu Jan 06, 2011 11:40 pm
-
Location:Near New Orleans
Pass your cutting torch closely over some 100* steel, and see the band of water droplets on each side of your path. My point is, the water didn't come out of the steel, it came from the flame.
Steve S
Steve S
jwmacawful
- jwmacawful
-
Heavy Hitter
-
Posts:
-
Joined:Fri Aug 13, 2010 1:23 pm
-
Location:the city that never sleeps
- MinnesotaDave
-
Weldmonger
-
Posts:
-
Joined:Sun Oct 27, 2013 10:57 pm
-
Location:Big Lake/Monticello MN, U.S.A.
Strange statement jwmacawful.jwmacawful wrote:steel retains moisture during climate change. it's called dew point. preheat removes this.
"The dewpoint temperature is the temperature at which the air can no longer "hold" all of the water vapor which is mixed with it, and some of the water vapor must condense into liquid water. The dew point is always lower than (or equal to) the air temperature"
http://www.weatherquestions.com/What_is ... rature.htm
It is my understanding that the water droplets on the surface of steel do not come from the steel itself.
The water condenses on the surface much like it does on a pop can.
The water can come from the torch, the air, or a combination of both.
Never seen a moisture meter to check if the steel is "waterlogged."
Preheat temps and interpass temps are about the way steel grain structure behaves during welding.
I'm not a science genius, so I'll leave the technical explanation to others.
http://www.aisc.org/bookstore/itemredir ... x?id=14870
Dave J.
Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~
Syncro 350
Invertec v250-s
Thermal Arc 161 and 300
MM210
Dialarc
Tried being normal once, didn't take....I think it was a Tuesday.
Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~
Syncro 350
Invertec v250-s
Thermal Arc 161 and 300
MM210
Dialarc
Tried being normal once, didn't take....I think it was a Tuesday.
I was preheating some 1/2 inch alum plate prior to TIG welding it when I notice moisture forming on it. I was wondering where in the hell that came from? Now I know. That's funny.
Everlast PowerTig 250EX, PowerTig 185 Micro, PowerArc 160STH, Miller Trailblazer 301G, Millermatic 140 Auto-Set
- Otto Nobedder
-
Weldmonger
-
Posts:
-
Joined:Thu Jan 06, 2011 11:40 pm
-
Location:Near New Orleans
jwmacawfull,
A water molecule is simply too large to work it's way in to steel. To make steel, you have to heat it to extreme temperatures to get it to accept carbon atoms.
I detect vacuum leaks by finding where Helium atoms, one of the smallest things in "normal" nature can pass. I can often temporarily plug these leaks with water, because it can't pass through.
Steel is not porous to water. Someone pulled your leg once, to get you to do it his way.
Steve S
A water molecule is simply too large to work it's way in to steel. To make steel, you have to heat it to extreme temperatures to get it to accept carbon atoms.
I detect vacuum leaks by finding where Helium atoms, one of the smallest things in "normal" nature can pass. I can often temporarily plug these leaks with water, because it can't pass through.
Steel is not porous to water. Someone pulled your leg once, to get you to do it his way.
Steve S
jwmacawful
- jwmacawful
-
Heavy Hitter
-
Posts:
-
Joined:Fri Aug 13, 2010 1:23 pm
-
Location:the city that never sleeps
oddo nobetter/steveOtto Nobedder wrote:jwmacawfull,
A water molecule is simply too large to work it's way in to steel. To make steel, you have to heat it to extreme temperatures to get it to accept carbon atoms.
I detect vacuum leaks by finding where Helium atoms, one of the smallest things in "normal" nature can pass. I can often temporarily plug these leaks with water, because it can't pass through.
Steel is not porous to water. Someone pulled your leg once, to get you to do it his way.
Steve S
who said the water was inside the steel?? this is SURFACE water that is called condensation. it is the same principal as putting cold beer in a warm glass. the droplets that form on the outside of the glass isn't beer. the glass isn't leaking. same principal. raising the temp of the steel above the dew point prevents the water that is on the surface of that steel from condensing. the only one pulling my leg is you. what a joker you are!!
- Otto Nobedder
-
Weldmonger
-
Posts:
-
Joined:Thu Jan 06, 2011 11:40 pm
-
Location:Near New Orleans
jwmacawful
- jwmacawful
-
Heavy Hitter
-
Posts:
-
Joined:Fri Aug 13, 2010 1:23 pm
-
Location:the city that never sleeps
simple physics. but if you have to be right you gotta expect to be teased for it.Otto Nobedder wrote:You're enjoying this WAY to much.
That tells me I'm probably being teased here.
Steve S
- Otto Nobedder
-
Weldmonger
-
Posts:
-
Joined:Thu Jan 06, 2011 11:40 pm
-
Location:Near New Orleans
The condensation on your beer glass came out of the air, not the glass, to use your analogy
That was fun. And I don't mind being challenged. I've been wrong once or twice .
Steve S
That was fun. And I don't mind being challenged. I've been wrong once or twice .
Steve S
jwmacawful
- jwmacawful
-
Heavy Hitter
-
Posts:
-
Joined:Fri Aug 13, 2010 1:23 pm
-
Location:the city that never sleeps
now you got it. the same way the water is condensing on the steel. from the air. i knew if i used beer.....Otto Nobedder wrote:The condensation on your beer glass came out of the air, not the glass, to use your analogy
That was fun. And I don't mind being challenged. I've been wrong once or twice .
Steve S
Return to “Stick Welding/Arc Welding - Shielded Metal Arc Welding”
Jump to
- Introductions & How to Use the Forum
- ↳ Welcome!
- ↳ Member Introductions
- ↳ How to Use the Forum
- ↳ Moderator Applications
- Welding Discussion
- ↳ Metal Cutting
- ↳ Tig Welding - Tig Welding Aluminum - Tig Welding Techniques - Aluminum Tig Welding
- ↳ Mig and Flux Core - gas metal arc welding & flux cored arc welding
- ↳ Stick Welding/Arc Welding - Shielded Metal Arc Welding
- ↳ Welding Forum General Shop Talk
- ↳ Welding Certification - Stick/Arc Welding, Tig Welding, Mig Welding Certification tests - Welding Tests of all kinds
- ↳ Welding Projects - Welding project Ideas - Welding project plans
- ↳ Product Reviews
- ↳ Fuel Gas Heating
- Welding Tips & Tricks
- ↳ Video Discussion
- ↳ Wish List
- Announcements & Feedback
- ↳ Forum News
- ↳ Suggestions, Feedback and Support
- Welding Marketplace
- ↳ Welding Jobs - Industrial Welding Jobs - Pipe Welding Jobs - Tig Welding Jobs
- ↳ Classifieds - Buy, Sell, Trade Used Welding Equipment
- Welding Resources
- ↳ Tradeshows, Seminars and Events
- ↳ The Welding Library
- ↳ Education Opportunities