Tig welding tips, questions, equipment, applications, instructions, techniques, tig welding machines, troubleshooting tig welding process
Post Reply
Raffus
  • Posts:
  • Joined:
    Tue Dec 30, 2014 4:38 pm

What causes this
Everlast 210 ext.
setup
130 amps
Ac balance 30
Ac frequency (hz) 120
30 scfh argon
Attachments
image.jpg
image.jpg (43.39 KiB) Viewed 423 times
Artie F. Emm
  • Posts:
  • Joined:
    Thu Jul 24, 2014 7:53 am

I'm wondering if your argon flow rate is too high. The Miller welding calculator,
http://www.millerwelds.com/resources/ca ... ulator.php
suggests 17 cfh. I'm not sure that will solve the problem but it will make your bottle last longer. ;)
Dave
aka "RTFM"
User avatar
  • Posts:
  • Joined:
    Thu Jan 24, 2013 6:44 am

Yes, much too high. The end of the piece could be causing additional turbulence resulting in what you are seeing in the weld.
Post Reply