So now I've started practicing T joints & am failing miserably. My self diagnosis is drawing a blank (with respect to what I am doing wrong & what needs to change) on this T joint.
Setup:
- 1/8" carbon steel - T joint
- 115 AMPs on the foot pedal (I normally use 100 AMPs on a butt joint, which seems plenty good enough)
- 3/32" - 2% lanthanated tungsten
- #8 cup
- 1/16" filler wire - ER70S-2
- approx 20 CFM argon
Generally, my past problems (on other welds) are not enough AMPs or moving torch too fast and losing control of the weld puddle. Is that my problem(s) here ?