Laser work
Posted: Tue Jan 24, 2017 4:05 pm
I was wondering if anyone out there has done any mixed metal laser welding?
I have welded most common tool steels with similar filler metals. I have welded most tool steels with 420ss filler.
I would like to increase the surface hardness of a standard H13 ejector pin in a certain area. I would think M2 would give me a good hard surface if compatible. I would use .010" filler and shoot for at least .008" to .010" finished thickness.
Maybe A2.
I will try both, I was just curious what the welding world has to say.
Fats
I have welded most common tool steels with similar filler metals. I have welded most tool steels with 420ss filler.
I would like to increase the surface hardness of a standard H13 ejector pin in a certain area. I would think M2 would give me a good hard surface if compatible. I would use .010" filler and shoot for at least .008" to .010" finished thickness.
Maybe A2.
I will try both, I was just curious what the welding world has to say.
Fats