Tig welding tips, questions, equipment, applications, instructions, techniques, tig welding machines, troubleshooting tig welding process
Post Reply
motox
  • Posts:
  • Joined:
    Thu Nov 28, 2013 12:49 pm
  • Location:
    Delaware

i think the basic rule for tig is a degree per thousandth for steel but what would you
use as a base number for silicon bronze tig or is this a redundant question?
htp invertig 221
syncrowave 250
miller 140 mig
hypertherm plasma
morse 14 metal devil
User avatar
  • Posts:
  • Joined:
    Thu Jan 24, 2013 6:44 am

I would say 2/3 to 3/4 of what you would use to weld.
User avatar
  • Posts:
  • Joined:
    Thu Dec 26, 2013 12:41 am
  • Location:
    Laredo, Tx

zank wrote:I would say 2/3 to 3/4 of what you would use to weld.
Yup, it still has to get red-hot so that sounds about right.
Image
motox
  • Posts:
  • Joined:
    Thu Nov 28, 2013 12:49 pm
  • Location:
    Delaware

thanks for the helpful input
htp invertig 221
syncrowave 250
miller 140 mig
hypertherm plasma
morse 14 metal devil
Post Reply